304 stainless steel pipe is a more common type of stainless steel materials, many of the processing plant, 304 stainless steel pipe may occur in the process of machining line crack, scarring, surface defects such as inclusions, and scarring, these defects is roughly due to slab outer arc Angle of subcutaneous appeared transverse crack, there are tiny impurities mixed with in the crystallizer, finishing clean up without oxidation residue on the surface of the stainless steel pipe, as well as in the rolling process due to slab edges to the stainless steel pipe surface caused by the cartwheel.
These defects not only lower the quality of the surface of the stainless steel pipe, also had an impact to the ascension of the quality of the product, so do a good job in prevention and treatment of 304 stainless steel pipe surface defects is very important.
304 stainless steel pipe billet surface deep scratches because the roll fan-shaped section of the local rotation, in order to prevent this happening, to timely maintenance in the fan section, it is strictly prohibited equipment over age. If the crystallizer with tiny impurities mixed with can cause the change of water quality, so to regularly check for water samples of mold. Reduce the weakening of stainless steel plate edge crack width to the extent and inhomogeneous deformation of wide plate rolling edge, reduce the amount of bandwidth when rolling steel plate is the best method, that is to say as far as possible with the wide end face slab width of steel plate production.
Prevent 304 stainless steel pipe in the process of bending of the slab corner into the brittleness temperature zone, so for different width of face slab corner for dynamic temperature control, control and implementation of bending section with water area. Reduce the uneven deformation of rolled piece in will reduce the rolled piece on the difference of deformation resistance below, optimize the billet reheating process, reduce the slab surface temperature difference. Prevent the depth of the local burn mark and clear clean after finishing the secondary defects such as slab surface oxidation slag, through improve the slab sizing ability of 304 stainless steel pipe.
Source: wilsonpipeline Pipe Industry Co., Limited (www.wilsonpipeline.com)
Tuesday, January 4, 2022
The causes of cracks in the 304 stainless steel pipe in the processing
Related Posts:
What is a Stainless Steel Flange?Metal flanges are common in numerous applications, but under certain circumstances, some types of metal flanges are better than others. A flange assem… Read More
Duplex and Super DuplexDuplex Duplex is a material that has approximately equal amounts of austenite and ferrite. These combine excellent corrosion resistance with high stre… Read More
Chemical Composition List For Special Austenitic GradesChemical Composition List For Special Austenitic GradesDesignationChemical composition % by mass max unless statedUNS NoSAE NoAISI No / Common NameCSi… Read More
Chemical Composition List For General Stainless Steel GradeChemical Composition List For General Stainless Steel Grade: DesignationChemical composition % by mass max unless statedUNS NoSAE NoAISI No / Common N… Read More
What Are the Different Types of Metal Flanges?Commonly found in plumbing applications, metal flanges provide a quick and easy method for joining lengths of pipe to one another. A flange consists o… Read More
Standard Reference for Seamless Steel Pipe
1. Seamless steel tube for structure (GB / T8162-1999) is a seamless steel pipe for general structure and mechanical structure. 2. Seamles...