ASME B 16.5-2003 CLASS 400 | ||||||||||||
CLASS 400 | FLANGE | LTB | DRILLINE DATA | CLASS 400 | ||||||||
NOMINAL | FLANGE | THICKNESS | BOSSED | WELD | LAP JOINT | LONG | PITCH | BOLT | NUMBER | NOMINAL | ||
MM | INCH | OD | T & T1 | L | L1 | L2 | L3 | PCD | H | # | MM | INCH |
15 | 1/2 | 95 | 14.3 | 29 | 59 | 22 | 229 | 66.7 | 16 | 4 | 15 | 1/2 |
20 | 3/4 | 115 | 15.9 | 32 | 64 | 25 | 229 | 82.6 | 20 | 4 | 20 | 3/4 |
25 | 1 | 125 | 17.5 | 34 | 69 | 27 | 229 | 88.9 | 20 | 4 | 25 | 1 |
32 | 1 1/4 | 135 | 20.7 | 36 | 74 | 29 | 229 | 98.4 | 20 | 4 | 32 | 1 1/4 |
40 | 1 1/2 | 155 | 22.3 | 39 | 77 | 32 | 229 | 114.3 | 22 | 4 | 40 | 1 1/2 |
50 | 2 | 165 | 25.4 | 44 | 80 | 37 | 229 | 127 | 20 | 8 | 50 | 2 |
65 | 2 1/2 | 190 | 28.6 | 48 | 86 | 41 | 229 | 149.2 | 22 | 8 | 65 | 2 1/2 |
80 | 3 | 210 | 31.8 | 53 | 90 | 46 | 229 | 168.3 | 22 | 8 | 80 | 3 |
90 | 3 1/2 | 230 | 35 | 56 | 93 | 49 | 229 | 184.2 | 26 | 8 | 90 | 3 1/2 |
100 | 4 | 255 | 35 | 58 | 96 | 51 | 229 | 200 | 26 | 8 | 100 | 4 |
125 | 5 | 280 | 38.1 | 61 | 109 | 54 | 305 | 235 | 26 | 8 | 125 | 5 |
150 | 6 | 320 | 41.3 | 64 | 110 | 57 | 305 | 269.9 | 26 | 12 | 150 | 6 |
200 | 8 | 380 | 47.7 | 75 | 124 | 68 | 305 | 330 | 30 | 12 | 200 | 8 |
250 | 10 | 445 | 54 | 80 | 131 | 102 | 305 | 387.5 | 32 | 16 | 250 | 10 |
300 | 12 | 520 | 57.2 | 86 | 144 | 108 | 305 | 450.8 | 35 | 16 | 300 | 12 |
350 | 14 | 585 | 60.4 | 91 | 156 | 117 | 305 | 514.4 | 35 | 20 | 350 | 14 |
400 | 16 | 650 | 63.5 | 101 | 159 | 127 | 305 | 571.5 | 38 | 20 | 400 | 16 |
450 | 18 | 710 | 66.7 | 105 | 172 | 137 | 305 | 628.6 | 38 | 24 | 450 | 18 |
500 | 20 | 775 | 69.9 | 109 | 175 | 146 | 305 | 685.8 | 42 | 24 | 500 | 20 |
600 | 24 | 915 | 76.2 | 121 | 182 | 159 | 305 | 812.8 | 48 | 24 | 600 | 24 |
NOTES:*Schedule of weld neck to be indicated. |
Tuesday, January 4, 2022
ASME B 16.5-2003 CLASS 400
Related Posts:
Selection of Stainless Steel Corrosion Resistance By wilsonpipeline.comStainless steel react with corrosive deterioration phenomenon is known as corrosion. Common metal corrosion of intergranular corrosion, pitting corros… Read More
Using Coatings to Extend the Life of Oil and Gas Pipeline ValvesIn the oil and gas industries, valves are key components involved in the control of the flow of corrosive, abrasive and erosive gases and fluids. Howe… Read More
How Does Offshore Stainless Steel Pipeline Installation Work?Laying pipe on the seafloor can pose a number of challenges, especially if the water is deep. There are three main ways that subsea stainless steel pi… Read More
Undersea Stainless Steel Pipeline History and Uses By wilsonpipeline.comThe first major undersea stainless steel pipeline was built during World War II. Nicknamed Operation PLUTO (Pipe Line Under The Ocean), this stainless… Read More
Use of Subsea Stainless Steel Pipeline By wilsonpipeline.comOne of the first major subsea stainless steel pipeline was built between Great Britain’s Isle of Wight and the coast of France during World War II an… Read More
Standard Reference for Seamless Steel Pipe
1. Seamless steel tube for structure (GB / T8162-1999) is a seamless steel pipe for general structure and mechanical structure. 2. Seamles...

0 comments:
Post a Comment